• Hafnium oxide obtained by atomic layer deposition technology promotes early osteogenesis via activation of Runx2-OPN-mir21A axis while inhibits osteoclasts activity

    12 days ago - By Journal of Nanobiotechnology

    Due to increasing aging of population prevalence of age-related disorders including osteoporosis is rapidly growing. Due to health and economic impact of the disease, there is an urgent need to develop techniq...